Wait time

Post by LCS »

How long do I have to wait after a full fused piece can be draped?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wait time

Post by Brad Walker »

Do you mean how long after it cools to room temperature or something else?
LCS
Posts: 8
Joined: Mon Aug 20, 2007 9:44 am

Re: Wait time

Post by LCS »

Yes ... after it cools to room temperature.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wait time

Post by Brad Walker »

If you wait until it cools, you can slump or drape immediately if you wish.
LCS
Posts: 8
Joined: Mon Aug 20, 2007 9:44 am

Re: Wait time

Post by LCS »

THANK YOU!