I was just looking at Bullseye’s ‘River Rock’ tutorial and want to try it. It calls for Sunset Coral powder, but I wondered if it would work with fine frit. (for me, more versatile than powder.)

http://www.bullseyeglass.com/methods-id ... ction.html

Also, would this work with other colors that react with French vanilla?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Bullseye ‘River Rock’ technique

Post by Brad Walker »

It would work with lots of other colors that react. It will work much better with powder than with fine frit.