Hi fusers, the glass lens for the peep hole in my kiln is worn and blurry. I successfully removed it from the fire brick holding it. It is 3" square quartz, 1/4" thick. I don't know how to replace it, as the manufacturer has stopped making this kiln. (L and L). So, they don't have parts. Any thoughts as to where I ca get a replacement? Thanks!
Bonnie Rubinstein
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Replacing Glass for peep hole

Post by Brad Walker »

Replace it with a brick. Kiln brick is soft enough that you could carve to ship and place in the hole where the quartz glass was.

If you absolutely have to have the quartz window (not sure why!), there are companies that can cut you a piece to size. Try https://technicalglass.com/product_page ... tes_discs/ or Google for others.
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Replacing Glass for peep hole

Post by Bonnie Rubinstein »

Hi Brad,
Thanks! I see they do have the size I need- that was very useful info!

I have the brick, I just need to slide the right sized glass into the slot for it. I need to watch the progress of the fuse, and the glass makes it easier..