Hxtal and HYG adhesives
Moderators: Brad Walker, Tony Smith
-
flite risk
- Posts: 5
- Joined: Sat Mar 04, 2006 10:54 am
- Location: Hamilton, MT
Hxtal and HYG adhesives
Hi all. I have always used mechanical means to attach my glass to other mediums but want to start using adhesives because I am hoping it creates new opportunities with my artwork. I have Hxtal, Hang Your Glass and E6000 in my shop. I looked through the archives and it seems that Hxtal had the least failures for most of the folks that chimed in. I am aware of it's long setup time and that doesn't bother me as I am more concerned with bond failure than time. I have used the HYG and it sure seems to work quick and create a strong bond although some folks mentioned it yellows after time...which doesn't bother me either because I would hide the bond. I did read that some folks had some failure with it over time...which I don't want and is why I have been reluctant to use adhesives. I would appreciate opinions from folks that have used adhesives to bond metal (aluminum) to glass and glass to glass. As an experiment I have already bonded (Hxtal) some heavy glass pieces to a thick aluminum sheet and will be hanging it up to see how it does. Any input appreciated! Thanks
SDG
Re: Hxtal and HYG adhesives
Of the three I would only use hxtal and never the others. had problems with yellowing and failing. The only other I use, and I use it mostly for hanging hardware is loctite hysol h30cl. It is super for metal to glass, never yellows. Course if I have to cold work, it's back to hxtal
-
flite risk
- Posts: 5
- Joined: Sat Mar 04, 2006 10:54 am
- Location: Hamilton, MT
Re: Hxtal and HYG adhesives
Thanks for the input. I have never heard of Loctite hysol h30cl so will look it up. Thats exactly what I am looking for to adhere the glass directly to the aluminum. Thanks!Dick wrote:Of the three I would only use hxtal and never the others. had problems with yellowing and failing. The only other I use, and I use it mostly for hanging hardware is loctite hysol h30cl. It is super for metal to glass, never yellows. Course if I have to cold work, it's back to hxtal
SDG