Drop out firing schedule
Moderators: Brad Walker, Tony Smith
-
Doug Zawodny
- Posts: 33
- Joined: Wed Feb 28, 2007 8:30 pm
- Location: Sacramento California
Drop out firing schedule
First time trying a drop out. I have a 15 in x1/2 disk over a 8in hole. Any suggestions for a firing schedule. I’ll be watching the drop to stop at 8in.
-
Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Drop out firing schedule
Hold at 1250 to 1300 until done.