Fusing 5mm clear sheets

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Peter Zelle
Posts: 4
Joined: Tue May 01, 2007 10:58 pm

Fusing 5mm clear sheets

Post by Peter Zelle »

Hi,
I am running out of COE 96 casting plates and cannot find anymore. Sadness.
My castings are 6 to 7 feet tall and about 1.5 thick with frit on the surface of the mold.
Thinking of fusing 8 layers of 5mm clear sheets together.
Is this crazy or worth a try?
Appreciate any thoughts or info your can share,
Thanks, Peter
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Fusing 5mm clear sheets

Post by Kevin Midgley »

Switch to Bullseye glass.
Yes you can fuse sheets together however inevitably there will be bits of 'stuff like studio dust' between the layers.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: Fusing 5mm clear sheets

Post by Terry Gallentine »

Peter--Did you go ahead and experiment with fusing multiple layers of 5mm clear together? If you did, did you use the Oceanside 96 or did you use the Wissmach 96? I am thinking about trying out the Wissmach 96 and might be interested in putting together an order with someone else for some full sheets (32"x42").