Post by Terry Gallentine »

I am considering purchasing a three phase kiln but I would have to convert it to single phase for my shop. Does anyone out there have any experience doing this and what is involved in the process?
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Kiln Conversion

Post by Brad Walker »

Here's how Skutt does it: https://skutt.com/skutt-resources/repai ... e-of-kiln/