Bubble
Moderators: Brad Walker, Tony Smith
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Bubble
I'm sometimes getting a large bubble when fusing this piece, the long dimension is 12 inches. Fired on Papyros, my usual full-fuse program that works fine with smaller pieces, and sometimes works fine with this size. Any ideas what causes this?
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Re: Bubble
I think I found the answer ... right here on this website. I'll try adjusting my schedule.
https://warmglass.com/what-caused-this-huge-bubble/
https://warmglass.com/what-caused-this-huge-bubble/
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Bubble
Yep. I was just about the send you that link. Slow down, reduce top temperature.Eric Bloom wrote:I think I found the answer ... right here on this website. I'll try adjusting my schedule.
https://warmglass.com/what-caused-this-huge-bubble/