Any suggestions on how to apply a reflective backing or coating to flat fused glass?
Thank you.
reflective backing?
Moderators: Brad Walker, Tony Smith
-
Bonnie Rubinstein
- Posts: 236
- Joined: Sun May 04, 2003 9:04 pm
- Location: River Falls, WI
reflective backing?
Bonnie Rubinstein
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Re: reflective backing?
Rust-Oleum makes a spray paint for this. It gets applied to the back, after firing. Also needs a clear coat after the reflective finish is applied. Read and follow the directions. It doesn't give a mirror-like finish but it does reflect. It also seems to highlight every little imperfection in the glass.
-
Bonnie Rubinstein
- Posts: 236
- Joined: Sun May 04, 2003 9:04 pm
- Location: River Falls, WI
Re: reflective backing?
Terrific, thanks.
Do you think if I apply an adhesive to that final clear coat( to apply glass to another surface), it will not disturb the coatings?
Do you think if I apply an adhesive to that final clear coat( to apply glass to another surface), it will not disturb the coatings?
Bonnie Rubinstein
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Re: reflective backing?
If the adhesive will stick to a painted surface it might be OK. But if the adhesive instructions say to remove any paint, then it probably won't work.
Re: reflective backing?
Bonnie, depending where you live there might be a company in town that does silvering (mirror finish on glass), if you want a mirror-type reflection. There was a company in Vancouver,BC, Fish bros., I think, that would silver your glass for you. Good luck