reflective backing?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 236
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

reflective backing?

Post by Bonnie Rubinstein »

Any suggestions on how to apply a reflective backing or coating to flat fused glass?

Thank you.
Bonnie Rubinstein
Eric Bloom
Posts: 8
Joined: Fri May 15, 2020 3:39 pm

Re: reflective backing?

Post by Eric Bloom »

Rust-Oleum makes a spray paint for this. It gets applied to the back, after firing. Also needs a clear coat after the reflective finish is applied. Read and follow the directions. It doesn't give a mirror-like finish but it does reflect. It also seems to highlight every little imperfection in the glass.
IMG_4068.jpg
Bonnie Rubinstein
Posts: 236
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: reflective backing?

Post by Bonnie Rubinstein »

Terrific, thanks.
Do you think if I apply an adhesive to that final clear coat( to apply glass to another surface), it will not disturb the coatings?
Bonnie Rubinstein
Eric Bloom
Posts: 8
Joined: Fri May 15, 2020 3:39 pm

Re: reflective backing?

Post by Eric Bloom »

If the adhesive will stick to a painted surface it might be OK. But if the adhesive instructions say to remove any paint, then it probably won't work.
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: reflective backing?

Post by Buttercup »

Bonnie, depending where you live there might be a company in town that does silvering (mirror finish on glass), if you want a mirror-type reflection. There was a company in Vancouver,BC, Fish bros., I think, that would silver your glass for you. Good luck