Drop out temp

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Drop out temp

Post by Doug Zawodny »

Those out there doing drop outs, what is your high temp?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Drop out temp

Post by Brad Walker »

1300F. Never higher than 1325. Hold until drop is done.
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Re: Drop out temp

Post by Doug Zawodny »

Thank you.
Post Reply