Anneling kiln for fusing?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Anneling kiln for fusing?

Post by Bonnie Rubinstein »

Hi All,
I know someone who has a few annealing kilns for use by glass blowers. He wonders if they could also be used for fusing. I am not familiar with annealers.
Can they be also used for fusing?
Thanks!
Bonnie Rubinstein
Mark Hughes
Posts: 49
Joined: Mon Mar 17, 2003 6:27 pm
Location: Omaha, Nebraska

Re: Anneling kiln for fusing?

Post by Mark Hughes »

It should as long as it will fire to the processing temps you need for your work. The Skutt ones I looked at had a top temp of 1700*, which is higher than you need for Bullseye glass.
Mark Hughes
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Anneling kiln for fusing?

Post by Bonnie Rubinstein »

Thank you. he said it does go to 1400.

I should probably check to see what his controller looks like.
Bonnie Rubinstein
Post Reply