Top temperature for Ferro Sunshine enamels

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Maggie Abdel Rahman
Posts: 38
Joined: Tue Nov 06, 2007 10:16 am

Top temperature for Ferro Sunshine enamels

Post by Maggie Abdel Rahman »

Hello!
If you have used Ferro Sunshine enamels ...

what is the temperature required for the enamels to just ADHERE to glass?
the enamels will be applied to one sheet of float glass in a first firing.
I would aporeciate your recommendations
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Top temperature for Ferro Sunshine enamels

Post by Brad Walker »

We fire to just adhere to 1325F.

Note that some colors will not mature to final color at this temperature.

You can also add Mixing Flux to lower the temperature.
Maggie Abdel Rahman
Posts: 38
Joined: Tue Nov 06, 2007 10:16 am

Re: Top temperature for Ferro Sunshine enamels

Post by Maggie Abdel Rahman »

Thank you
Post Reply