Hello!
If you have used Ferro Sunshine enamels ...
what is the temperature required for the enamels to just ADHERE to glass?
the enamels will be applied to one sheet of float glass in a first firing.
I would aporeciate your recommendations
Top temperature for Ferro Sunshine enamels
Moderators: Brad Walker, Tony Smith
-
Maggie Abdel Rahman
- Posts: 38
- Joined: Tue Nov 06, 2007 10:16 am
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Top temperature for Ferro Sunshine enamels
We fire to just adhere to 1325F.
Note that some colors will not mature to final color at this temperature.
You can also add Mixing Flux to lower the temperature.
Note that some colors will not mature to final color at this temperature.
You can also add Mixing Flux to lower the temperature.
-