Researching large kilns

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bonnie Rubinstein
Posts: 237
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Researching large kilns

Post by Bonnie Rubinstein »

Hi All,

looking to find a large kiln for a workshop that I will teach. Anything 40" + in length would be great. Recommendations anyone?
Thank you.
Bonnie Rubinstein
Bonnie Rubinstein
Posts: 237
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Researching large kilns

Post by Bonnie Rubinstein »

I am looking for information about manufacturers of large kilns. I am leaning away from the fiber kilns, since I want more control over annealing stages, and they cool down too fast.
Do any of you use large kilns that you can recommend?
Bonnie Rubinstein
carol carson
Posts: 58
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Researching large kilns

Post by carol carson »

Are you looking to buy a large kiln? If so, how large?
Bonnie Rubinstein
Posts: 237
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Researching large kilns

Post by Bonnie Rubinstein »

Hi Carol,
Minimum 26" x 42".
Bonnie
Bonnie Rubinstein
carol carson
Posts: 58
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Researching large kilns

Post by carol carson »

Are you looking to buy?
I know of one (much larger than 26"x42") in Hillsboro Oregon, if you're interested.
Bonnie Rubinstein
Posts: 237
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Researching large kilns

Post by Bonnie Rubinstein »

yes, Carol, I am interested. Please message me with info; size, age, manufacturer, controller, etc.

Thank you
Bonnie Rubinstein
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Researching large kilns

Post by Buttercup »

Hi Bonnie,
If you don't find what you want ready-made do you have access to the resources to build one? This thread contains pictures of a lid rebuild to replace the elements for a top-fired kiln, the rest is just a fibre-lined brick box held together with angle-iron rods and bolts.

It was built for me by an electrician friend from a sketch I made of a top-fired brick kiln at Pilchuck (last century). It's still my favourite kiln.

viewtopic.php?p=354030&hilit=home+made#p354030
Bonnie Rubinstein
Posts: 237
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Researching large kilns

Post by Bonnie Rubinstein »

I am buying it on behalf of someone else who, turns out, only wants a new kiln from a reputable manufacturer. he has no interest in building one, but I appreciate the response you provided.
Bonnie Rubinstein
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Researching large kilns

Post by Buttercup »

You're welcome!
Post Reply