What to use on a 3mm piece of base and 3mm dichro
Moderators: Brad Walker, Tony Smith
-
Karen Avery
- Posts: 3
- Joined: Fri Nov 01, 2024 2:55 pm
What to use on a 3mm piece of base and 3mm dichro
I am going to make a plate with a base piece of 3mm black glass and a layer of 3mm dichro down the middle. I was planning on putting a 3mm piece of clear class over it all but am afraid of the space that is between the top and bottom pieces (the base and the cap). What can I put on the black glass before firing so that it doesn't make a lot of bubbles? I am going to slump it after so need to do a full fuse. It is System 96.
-
Brad Walker
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: What to use on a 3mm piece of base and 3mm dichro
Put the clear below the black, not on top.
-
Karen Avery
- Posts: 3
- Joined: Fri Nov 01, 2024 2:55 pm
Re: What to use on a 3mm piece of base and 3mm dichro
If I put it under the black, the dichro won't have any protection on it. I guess I will have to do that though.
-
Brad Walker
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: What to use on a 3mm piece of base and 3mm dichro
You can sift a very thin layer of clear powder (two grains thick at most) over the entire top of the piece.
Or use dichro on clear and fire upside down.
Or use dichro on clear and fire upside down.