rough surface on plate

Post by jolly »

After 25 years of fusing with window glass, I have been talked into using Bullseye glass. It is fun, I've always liked color but my first larger piece has an issue that I didn't expect. I used glass that I knew would react with each other and it turned out great but the stems on the flowers are rough and crusty feeling when I touch it. I have the ability to wet sand it and go through all the grits to polish before I slump it but is that what people who know this glass do when this happens? Seems like capping it with clear would make it really thick since it is only a 10 in x 10 inch square. Thanks.
There is more to life than increasing its speed.-Mahatma Gandhi
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: rough surface on plate

Post by Brad Walker »

You'll need to give us more information.

What glass? What firing schedule? Got a photo?
jolly
Posts: 67
Joined: Thu Jan 08, 2004 7:44 pm
Location: Port Townsend, WA

Re: rough surface on plate

Post by jolly »

I was able to fix it just by using a kitchen scrubby. It had a little crusty area on the stringers that reacted to the surface glass.
There is more to life than increasing its speed.-Mahatma Gandhi
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: rough surface on plate

Post by Kevin Midgley »

stringers are made by fully abusing the glass. devitrification may occur as a result. try firing to a lower temperature
some colours are more affected than others