wanting to learn glass weaving

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Gabriel
Posts: 28
Joined: Sat Apr 19, 2003 4:36 pm
Location: Fort Wayne, IN

wanting to learn glass weaving

Post by Gabriel »

I searched through the archives for "glass weaving" looking to match all term and was only able to find 3 threads. I quickly browsed through all of them, but did not find any links or relative information on how to acomplish this. Does anyone offer a glass, book, or web link that can give more insight into how this is done?

Thanks
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

glass weaving

Post by slats »

beautiful site brock but it doesnt explain how it is done.
Katia T.
Posts: 33
Joined: Sun Mar 23, 2003 4:35 pm
Location: Rio de Janeiro / Brazil

Re: glass weaving

Post by Katia T. »

doctac wrote:beautiful site brock but it doesnt explain how it is done.
This site has a picture of how it´s donne. I think it is amazing...
http://www.brottworks.com/woven.html?95,26
Katia
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: glass weaving

Post by Brock »

doctac wrote:beautiful site brock but it doesnt explain how it is done.
Contact Bill, and ask him!

Don't be surprised if you have to figure it out by yourself.

If I had spent a lot of time perfecting a technique, I may not just give it away!

Brock
My memory is so good, I can't remember the last time I forgot something . . .
travisraybold
Posts: 25
Joined: Tue Jan 20, 2004 12:10 pm
Location: Portland, OR
Contact:

Post by travisraybold »

i've never tried it, but i thought about making a wavy mold and slumping thin strips on it, then offsetting every other piece by half of the wavelength, and feeding straight strips through crosswise, then tack fusing the whole thing.

it might work :)

--travis
sadiesjewels
Posts: 48
Joined: Mon Mar 10, 2003 2:02 pm
Location: N. CA
Contact:

Post by sadiesjewels »

Hello ...

My understanding is this is how it is done - basics only as I've never done it myself ...

Cut some fiber paper/board strips ... say 1/8" thick fiber paper/board and lay them on a kiln shelf a suitable distance apart .. say 1" or so - all horizontal to each other ... then cut 3/4" strips of glass and slump them over the fiber paper/board so that the glass is effectively wavy in appearance. Now weave more 3/4" strips of glass through the wavy pieces (you have to offset them one space I think) ... now tack fuse them together ... so that you have a lattice.

Finally ... and this is the tricky part I think ... make some kind of mold to slump the lattice over - and the examples you see defy my non existent mold making skills ... perhaps he manipulates them hot? I think they are wonderful! Then slump or do whatever to make them into contorted wonderful lattice shapes ...

Or, just slump them into a ceramic bowl - smile ...

sadie


- I believe there was a thread on it sometime in the distant past ...
sadiesjewels
Posts: 48
Joined: Mon Mar 10, 2003 2:02 pm
Location: N. CA
Contact:

Post by sadiesjewels »

ahh ... so it really does help to read the whole thread and follow the links ... lol!

sadie
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Post by Jack Bowman »

sadiesjewels wrote:Hello ...

My understanding is this is how it is done - basics only as I've never done it myself ...

Cut some fiber paper/board strips ... say 1/8" thick fiber paper/board and lay them on a kiln shelf a suitable distance apart .. say 1" or so - all horizontal to each other .
I won't say 1/8" thick fiber won't work but it didn't work for me. I cut kiln shelves 3/8 to 1/2" thick and it worked. You have to take into account the thickness of the glass x2 plus the thickness of the glass you are going to insert. Anyway, that's what worked for me.

Jack
Andrew
Posts: 46
Joined: Fri Apr 11, 2003 1:39 pm
Location: Minnesota
Contact:

Jack's right

Post by Andrew »

Jack's right. I've made a weaving exactly that way. If you want to visualize it, draw an edge-on view. You have to account for the thickness of the glass when calculating how high to make the hills and valleys. I cut 1/2" fiberboard, and layed multiple pieces together on their sides then glued them at the right intervals to fiberpaper so they wouldn't move when I transferred them to the kiln. You have to make sure you put the glass on perpendicular to the cross pieces too.

You also need to fire it fairly hot because you are not just slumping but conforming some fairly lightweight pieces to your mold.

I haven't tried it, but glass noodles should work well and give a tighter weave.

Andy
Gabriel
Posts: 28
Joined: Sat Apr 19, 2003 4:36 pm
Location: Fort Wayne, IN

artists contacted

Post by Gabriel »

Just to update if anyone else is interested:
I contacted Andrew Brott and William Zweifel and neither are open to classes or one on one instruction at this moment. Andrew may be open to teaching classes at the earliest two quarters from now. I am going to speak to Roy at Delphi to see if that is a possibility.
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

Travis put it the most succinctly. I have been weaving for a while now, but have gotten more intense about it in the past two years. Like alot of techniques there is more than one way to do it, and the basics are not very difficult. Fiber board, brick, or pipes will serve as good form material for your first experiments. The challenge for me lies in getting good control of the process. It is not very hard to weave, but it is considerably harder to get good regularity and evenness. Lots of fun for weft brained individuals.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Tony Serviente wrote:Travis put it the most succinctly. I have been weaving for a while now, but have gotten more intense about it in the past two years. Like alot of techniques there is more than one way to do it, and the basics are not very difficult. Fiber board, brick, or pipes will serve as good form material for your first experiments. The challenge for me lies in getting good control of the process. It is not very hard to weave, but it is considerably harder to get good regularity and evenness. Lots of fun for weft brained individuals.
I just hope they're not warped. Brock
My memory is so good, I can't remember the last time I forgot something . . .
gone

Post by gone »

Brock wrote:
Tony Serviente wrote:Travis put it the most succinctly. I have been weaving for a while now, but have gotten more intense about it in the past two years. Like alot of techniques there is more than one way to do it, and the basics are not very difficult. Fiber board, brick, or pipes will serve as good form material for your first experiments. The challenge for me lies in getting good control of the process. It is not very hard to weave, but it is considerably harder to get good regularity and evenness. Lots of fun for weft brained individuals.
I just hope they're not warped. Brock
Ooooh, good one Brock!
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

Brock-Had to knit my brows for a good response, but at this point am suffering from shear tiredness and am just spinning my wheels. Maybe tomorrow there will be loom for improvement.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Tony Serviente wrote:Brock-Had to knit my brows for a good response, but at this point am suffering from shear tiredness and am just spinning my wheels. Maybe tomorrow there will be loom for improvement.
I feel enmeshed in an imbroglio here. I'm dyeing to get to the resolution of this, I can feel it in every fiber of my being, but I don't want to get fleeced. My car is a beater, and getting rid of it will be a big weight off my shoulders

I'm so happy, I'm beaming, because I got carded.

Rapunzel
My memory is so good, I can't remember the last time I forgot something . . .
froggee501
Posts: 43
Joined: Thu Feb 26, 2004 6:45 pm
Location: Portamazoo, MI

Post by froggee501 »

*groaning*

*loudly*

y'all are evil... :p
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

That sounds like a tale made of whole cloth. Wool do everyone a favor if we cut this out Brock. Ewe are as bad as I. Weave mutilated and spindled , and it is time to hold this topic at yarns length.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Tony Serviente wrote:That sounds like a tale made of whole cloth. Wool do everyone a favor if we cut this out Brock. Ewe are as bad as I. Weave mutilated and spindled , and it is time to hold this topic at yarns length.
Okay, Tony. I ran out of material anyway.

Skein of you to offer to end this.

Seams reasonable to me.

Brock
My memory is so good, I can't remember the last time I forgot something . . .
Bev Brandt
Posts: 50
Joined: Mon Mar 10, 2003 11:35 am
Location: St. Louis, MO
Contact:

Post by Bev Brandt »

Brock wrote:
Okay, Tony. I ran out of material anyway.

Skein of you to offer to end this.

Seams reasonable to me.

Brock
I guess it's too late to selvedge this thread. Maybe I'm biased, but it really ripped me up!

- Bev
Bev Brandt
Post Reply