Having been inspired by all the high fire and pot melt posts recently I have made some quite interesting pieces, however cutting them into circles seems to be a tricky. The one I cut today was 3/8th inches in thickness with a diameter of 16 inches. I used the little circle cutter device which came adrift three times during the cutting process. Cutting was very slow and I didn't think I was going to make it to the end of the cut without some sort of disaster, I didn't want to push it too hard in case I broke the blade.
If anyone has any advice on cutting thick circles I'd be very grateful to hear from you.
Best wishes
Linda
Thick cuts with Taurus 11
Moderators: Brad Walker, Tony Smith
-
Linda Denli
- Posts: 21
- Joined: Wed Aug 27, 2003 2:58 pm
- Location: London, UK
Thick cuts with Taurus 11
Linda from London
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I'm heartened to hear that it can work with the right touch. I suggest that you need a good pair of pliers that are designed for cutting thicker glass, the right cutter (134º angle wheel). Oh yeah, I'd use kerosene here just to be safer. Mineral spirits will evaporate before you are done.Brock wrote:I cut them by hand, but it's not for everybody, i guess. Brock
Brock, is your strategy to cut a circle 1" larger all around and then plier the score along to run it? I would probably take that approach with glass that is not transparent.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
I'm heartened to hear that it can work with the right touch. I suggest that you need a good pair of pliers that are designed for cutting thicker glass, the right cutter (134º angle wheel). Oh yeah, I'd use kerosene here just to be safer. Mineral spirits will evaporate before you are done.Bert Weiss wrote:Brock wrote:I cut them by hand, but it's not for everybody, i guess. Brock
Brock, is your strategy to cut a circle 1" larger all around and then plier the score along to run it? I would probably take that approach with glass that is not transparent.[/quote
Yup! I haven't ever had a problem with this method, but I make sure I get a good solid score, then just snap away the excess. I don't have professional tools for this, just my normal stuff. It works, but ya gotta believe! Brock
My memory is so good, I can't remember the last time I forgot something . . .