I made about a dozen 1" x 2" tiles of each of the following colors:
Red
Poppy
Manderine
orange
*also, lemon (very yellow), chestnut (dark brown) and ochre (tan)
(I fired to 1450/10 min)
Are the ugly 'brown' ones the red? (think dull brick red)
*should I have fired higher for the red?
Is Poppy really really bright reddish/orange
*these are really pretty!
Are orange and manderine really close? (these are the two that are confusing me the most)
One is lighter (more yellow?) the other is closer to poppy but still orange.
I know a manderine is an orange but is it darker than regular orange?
FYI/no comment needed... another no-no I did..... after I painted all the tiles, I had left over paint and painted some of the tiles by combining the left over paints - without writing down which paints I combined. Most of these are streaky so I know they are combos.
I will never do that (not take notes) again!
thanks,
g-