Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable
Thanks Randy

-
Brock
- Posts: 1519
- Joined: Mon Mar 10, 2003 1:32 pm
- Location: Vancouver, B.C.
Post
by Brock »
nbaybear wrote:Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable
Thanks Randy

Compatability won't be a problem, but what is this stuff? If it's real nacre, it's just gonna burn up. Maybe they're another form of mica? Brock
My memory is so good, I can't remember the last time I forgot something . . .
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Post
by Ron Coleman »
If the Mother of Pearl powders are the ones from CR Loo, they will work.
Just another name for mica powders.