I have made some cool things out of float  in my 18" kiln and they turned out great. However, I have  started using  a large kiln 9' x 4' ( shouldn't make any difference) but i tried to use the  following schedule t to slump 1/4 " float.
350h/1000 - 10min
700-1375 - 20 min
hold 1000 - 2 hours
I opened it up and not a damn thing but a minute movement on the edges. Do I need to go higher on this process or do you think my new kiln is just not functioning? I fused some bullseye in it the time before and it wa s perfect????
Any comments would be helpful.
Also Ive been searching around for scheduled for float. If anybody has any that they wouldnt mind sharing .......
Regards,
Sandy
			
			
									
						
										
						Float Sched. - Need Help
Moderators: Brad Walker, Tony Smith
- 
				Sandy Jackson
 - Posts: 10
 - Joined: Sun Mar 21, 2004 4:49 pm
 - Location: Denver
 - Contact:
 
- 
				Barbara Cashman
 - Posts: 151
 - Joined: Sun Mar 09, 2003 5:42 pm
 - Location: Greensboro NC
 - Contact:
 
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Float Sched. - Need Help
sandySandy Jackson wrote:I have made some cool things out of float in my 18" kiln and they turned out great. However, I have started using a large kiln 9' x 4' ( shouldn't make any difference) but i tried to use the following schedule t to slump 1/4 " float.
350h/1000 - 10min
700-1375 - 20 min
hold 1000 - 2 hours
I opened it up and not a damn thing but a minute movement on the edges. Do I need to go higher on this process or do you think my new kiln is just not functioning? I fused some bullseye in it the time before and it wa s perfect????
Any comments would be helpful.
Also Ive been searching around for scheduled for float. If anybody has any that they wouldnt mind sharing .......
Regards,
Sandy
In theory, 1375 should do the trick. So my first question is where is the thermocouple? Maybe it is too close to the elements.
You have 2 zones don't you? How are they set up control wise?
In my kiln, I would go up 600 dph to 1200, soak there for 20 minutes and then go to 1350 at maybe 400 dph and then soak for 10 or 20 minutes. Then I would fall to 1000 hold for 36 minutes take 36 minutes down to 900 then take 24 minutes down to 700 and 24 minutes down to 300 and crack the kiln when it actually reaches 300.
A slump test is always a good idea to determine what temp to anneal your glasses. In my kiln float slumped at 1100 so I anneal soak at 1000. Read up on the details of how to setup and do the slump test. I got it from Lundstrom Fusing book 1. I have posted in detail the process before.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Sandy Jackson
 - Posts: 10
 - Joined: Sun Mar 21, 2004 4:49 pm
 - Location: Denver
 - Contact: