Want to use it have bottle but directions partially rubbed off??? Warning label in front isnt I know to wear gloves, respirator. Directions would be helpful
Thanks Attie
Lauri Levanto
Posts: 270 Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland
Post
by Lauri Levanto » Fri Apr 16, 2004 2:27 pm
Don't even try
before you got proper safety instructions and equipment
-lauri
Tony Serviente
Posts: 328 Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:
Post
by Tony Serviente » Fri Apr 16, 2004 2:27 pm
Eye protection too! Put the bottle in warm water, in a disposable containter, as it will etch faster when warm. Brush on glass, wait 5 minutes, though more will not do any harm. Wash off with copious amounts of water. Don't forget that this cream works best on clear glass, and doing thin lines. If you etch broad areas it will look streaky, and it does not touch flashed. On colored cathedral glass the effects are very subtle. Have fun, be careful.
Kelly & Charlie MacMu
Post
by Kelly & Charlie MacMu » Fri Apr 16, 2004 2:34 pm
Do I fire my piece first or does this even matter?
Thanks
Ron Coleman
Posts: 468 Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA
Post
by Ron Coleman » Fri Apr 16, 2004 2:42 pm
Atticus wrote: Do I fire my piece first or does this even matter?
Thanks
Do any firing first and then etch after if you want the etching to stay.
Instructions, follow the link.
http://www.armourproducts.com/help/
Kelly & Charlie MacMu
Post
by Kelly & Charlie MacMu » Fri Apr 16, 2004 5:49 pm
Thanks Ron !
I went on google before I posted question and looked under armour glass etching cream all I found was where to buy it!
Thanks
vblue
Posts: 98 Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas
Post
by vblue » Fri Apr 16, 2004 5:52 pm
How long you leave the Armour Etch on depends on the glass. Don't leave it more than 30 seconds with dichroic and one of the "Rub 'n Etch" stencils.
I etched this piece of dichroic, capped it with clear and then fused.
I have more info on etching in my "Chemical Etching" album if you want to know about making your own stencils, etching on ceramic tiles, etc.
http://www.picturetrail.com/vernelle
Vernelle
Lauri Levanto
Posts: 270 Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland
Post
by Lauri Levanto » Sat Apr 17, 2004 1:32 am
Great page you have about etching.
May I include a link to it in the dictionary?
-lauri
vblue
Posts: 98 Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas
Post
by vblue » Sat Apr 17, 2004 6:36 am
Lauri,
What a nice compliment and great way to start the morning.
My Picture Trail albums are there to share ideas and help others. If you think the chemical etching album will help others, feel free to use it.
Vernelle
By the way, THANK YOU and Brad for all the work you are putting into creating the dictionary. It will be a valuable asset to everyone.
Kelly & Charlie MacMu
Post
by Kelly & Charlie MacMu » Sat Apr 17, 2004 12:28 pm
VBLUE THANKS !!!
Your site is outstanding!!! I love your work!!!
Thanks Attie