hole in pot melt

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Linda Hassur
Posts: 44
Joined: Sat Mar 15, 2003 10:40 pm

hole in pot melt

Post by Linda Hassur »

Some time ago, someone told what they used to keep the verticle pieces of glass from falling through the hole in the pot. I have searched the archives and have been unable to find that one particular post. Can anyone tell me what they did? Thanks Linda
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

just use larger pieces. stack them sideways across the hole, or put a piece of clear over the hole and then load in your colors on top of it.
Post Reply