yes i have a stupid li'l marshmallow with an infinite control switch....i want to start working on pattern bars and thicker pieces.....but it heats up too quickly! on the lowest setting (min) it still heats up at somewhere around 500 degrees an hour...is there any way i can control the rate more? now i've just been turning it off, letting it sit and then turning it back on...i don't know if this uneven heating is bad or not, but it sure is a pain...
any suggestions welcome
peace
- lauren
controlling the firing rate of a quickfire...
Moderators: Brad Walker, Tony Smith
Quick-fire
Go to http://www.aaproducts.com/kilnPar120v.html they have an infinite switch for $49 that is made for the QuickFire kiln. It lets you control the heat..low...medium... high, works great for larger or thicker pieces.
karen
karen
quick fire
don't know why the link isn't working ..just go to aaproducts.com and click on the 120v kilns.. it's the second item shown..
karen
karen
-
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
Lauren, I found that annealing thicker pieces in my quickfire was exceedingly difficult. When I used the quickfire (and I love it) I limited myself to small normal thickness pieces just because there was no way to control the annealing temperature. After several anneal breaks I decided that I should just work smaller till I got a larger kiln. Is there anywhere in your area where you can rent time on a larger kiln? That would be a way to get the thicker pieces made and annealed. Good luck!