how far over edge can I slump?
Moderators: Brad Walker, Tony Smith
how far over edge can I slump?
I have a blank that extends over the edge of a 15" bowl mold by 1/8 in and in some places 3/16 in. Can I slump into the mold and get away with it? I have a side fire kiln and am afraid the edges will droop down before the weight on the rest of the piece starts to slump pulling the edges into the bowl form. I am lazy and don't want to have to grind that much of the edge around such a large piece but will if I have to.
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Ann, I frequently have pieces hanging over the edge of my molds by up to 3/4" and they slump fine at 1150 without drooping. But, I am not sure how a side fire only kiln would do with that, maybe baffle around the piece to keep the edges from heating up too fast.
Lisa
Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
thank you all.
Appreciate the time you al took to respond. Ann