Flow temp for BE
Moderators: Brad Walker, Tony Smith
Flow temp for BE
Helen wants me to cast a couple pieces ....in non Pb glass.. so our glass choice is Bullseye ..crushed up sheets and scrap... my question is what is the flow temperature. for BE ( I haven't used BE for some time and have also lost all my records from previous firings for this glass)..Colin
-
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Re: Flow temp for BE
Bullseye starts moving for casting above 920 c (1700 f), at 980 c (1800 f) it flows nicely.Colin wrote: Helen wants me to cast a couple pieces ....in non Pb glass.. so our glass choice is Bullseye ..crushed up sheets and scrap... my question is what is the flow temperature. for BE ( I haven't used BE for some time and have also lost all my records from previous firings for this glass)..Colin
Ron
-
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact: