Custom grinder heads?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Custom grinder heads?

Post by Paul Tarlow »

Is there such a thing as a custom grinder head (for Glastar type grinders) or is it (reasonably) possible to make your own?

I need one that grinds 45 deg angles on small pieces. Do bevelers have a mechanism to get a relatively true and specific angle?

Thanks,
Paul
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

You can get anything "custom" but is it worth it? Better to rig up a jig to feed the work into the head at the angle you need.
watershed
Posts: 166
Joined: Wed Mar 12, 2003 1:44 am

Post by watershed »

There are lots of diamond, shaped bits. Whether they will fit your grinder? But probably the jig is a better option.

Greg

Oh I get mine from Harbor freight, they're just cheap. I don't use them enough to realize the cost/benefit from better ones, yet...
Jim Wixon
Posts: 35
Joined: Sun Mar 09, 2003 3:50 pm
Location: Seal Beach

Post by Jim Wixon »

Mika makes a 45º miter bit which will fit any of the common grinders.
http://www.sunshineglass.com has one.
jim
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Re: Custom grinder heads?

Post by Brian and Jenny Blanthorn »

Paul Tarlow wrote:Is there such a thing as a custom grinder head (for Glastar type grinders) or is it (reasonably) possible to make your own?

I need one that grinds 45 deg angles on small pieces. Do bevelers have a mechanism to get a relatively true and specific angle?

Thanks,
Paul
Bob over http://www.hisglassworks.com/index.html

I think has his own electroplating plant

If not he shure can help U out
Image
Post Reply