copper oxide

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Kay
Posts: 36
Joined: Wed Mar 12, 2003 4:20 pm
Location: Under Big Sky

copper oxide

Post by Kay »

O.K. Here I go again. Getting tired of me?
Reading the archives, it suggested mixing flux with copper oxide. In what proportions? Someone also suggested using borax to brighten the color. Guess this is another proportion :?
Having trouble with my hands keeping up with my head.
Kay
Brian and Jenny Blanthorn
Posts: 353
Joined: Mon Mar 10, 2003 5:25 pm
Location: UK
Contact:

Re: copper oxide

Post by Brian and Jenny Blanthorn »

Kay wrote:O.K. Here I go again. Getting tired of me?
Reading the archives, it suggested mixing flux with copper oxide. In what proportions? Someone also suggested using borax to brighten the color. Guess this is another proportion :?
Having trouble with my hands keeping up with my head.
Kay
Rather try real copper powder

Try 1 part flux 3 parts copper n also varie this

There hotter U go the more disolved but also the more problems ur gona get
Image