Here's an example of a happy accident! The mold broke during the slumping (don't know why!) but the result is quite cool......any comments?
http://aryana2.com/images/red_w_patern_ ... n_end2.jpg
Happy Accident!
Moderator: Brad Walker
-
- Posts: 8
- Joined: Sun Mar 09, 2003 11:22 pm
- Location: Cave Creek, AZ
- Contact:
Accident
That's a nice piece. Sometimes those accidents are great and the piece tells us what it wants to be. Without seeing your mold I can only guess why that happened, but it looks like the mold may have been thin in that area and gave way under the weight of the glass. That's just a guess.
Anyway, congrats, it's still a neat piece
Jerry
Anyway, congrats, it's still a neat piece
Jerry
-
- Posts: 8
- Joined: Sun Mar 09, 2003 11:22 pm
- Location: Cave Creek, AZ
- Contact:
happy accident
thanks for your compliment!
aryana
aryana
-
- Posts: 8
- Joined: Sun Mar 09, 2003 11:22 pm
- Location: Cave Creek, AZ
- Contact:
happy accident
hi, it's 11" diameter.......and thanks! it really was one of those cool kiln surprises....funny how every piece since then has been fusing and slumping perfectly since that sacrifice to the kiln god! ![Smile :)](./images/smilies/icon_smile.gif)