q-about rebuilding a top load kiln lid

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
dave laporta

q-about rebuilding a top load kiln lid

Post by dave laporta »

I have a crack running across my lid which I'll need to rebuild or replacefairly soon. So I have two questionsfor you: 1) should I build a new one myself OR purchase a replacement lid from the Manufacture? 2) if I consider building it myself (which I think can't be that hard) Are there any resources on;ine that might illustrate the steps or offer information? I will most likely upgrade to have elements in the lid if I do this.

My kiln is a Blue Diamond 23" side fire.

Any help would be most appreciated, thanks.
Dave
Clifford Ross
Posts: 68
Joined: Sun Mar 09, 2003 10:08 pm
Location: Myrtle Beach, So. Carolina
Contact:

Post by Clifford Ross »

Mortar the crack and tighten the outer band . No need for new lid yet.
noudegeest

Fixibg a kiln

Post by noudegeest »

I would contact Phil Teefy at Rainbow glassworks. he makes his own kilns and I don't think there is anything on the subject that he doesn't know. He also has the elements if you decided to put one's on the lid of your kiln. :shock:
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Post by Jack Bowman »

Do you have a link for Rainbow Glassworks?