Seeking Metal Foils
Moderators: Brad Walker, Tony Smith
- 
				fatcatglass
 
Seeking Metal Foils
I would like to find foil for inclusions (copper,silver,???)that is thicker than leaf but still thin enough to fuse.This is my first post and would appreciate any and all imput re:foil inclusions.....
Thanks,
Scott
			
			
									
						
										
						Thanks,
Scott
- 
				Judy Schnabel
 - Posts: 195
 - Joined: Mon Mar 10, 2003 9:45 pm
 - Location: SW FL
 - Contact:
 
Scott,
I hope this works
http://www.warmglass.com/cgi-bin/wgarchive3.pl?index
This is a link to a discussion in the archives regarding copper inclusions.
If this doesn't work, go to the archives and type in copper inclusions. There have been lots of discussions on different types of inclusions.
Judy
			
			
									
						
										
						I hope this works
http://www.warmglass.com/cgi-bin/wgarchive3.pl?index
This is a link to a discussion in the archives regarding copper inclusions.
If this doesn't work, go to the archives and type in copper inclusions. There have been lots of discussions on different types of inclusions.
Judy
- 
				Judy Schnabel
 - Posts: 195
 - Joined: Mon Mar 10, 2003 9:45 pm
 - Location: SW FL
 - Contact:
 
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
Olympic color rods sells all of the foils you mentioned http://www.glasscolor.com/catalog/metalLeaf/index.asp. 
The Bullseye connection http://www.bullseyeconnection.com also sells foil.
For copper screen, go to Michael's and buy the mesh used for moldmaking.
Tony
			
			
									
						
							The Bullseye connection http://www.bullseyeconnection.com also sells foil.
For copper screen, go to Michael's and buy the mesh used for moldmaking.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..."   Scott Berkun
			
						- 
				Cynthia
 
you can also try:
http://www.thompsonenamel.com
http://www.dickblick.com
Sepp Leaf products...1 800 971-7377
			
			
									
						
										
						http://www.thompsonenamel.com
http://www.dickblick.com
Sepp Leaf products...1 800 971-7377
- 
				Lisa Rivera Skubal
 - Posts: 2
 - Joined: Wed Mar 12, 2003 5:33 pm
 - Location: Washburn, Iowa
 
- 
				Tess Farley
 
Give a call to Jim Apistolas at Nimrod Hall Copper Company.  They carry copper sheeting in varying thickensses of 1 mil, 2 mil, 5 mil and 8 mil.  Widths are 6", 12" and 18".  Their number is 703-978-9192 or 703-447-6509.  Their email address is sales@nimrodhall.com.  They will send you some samples.
			
			
									
						
										
						- 
				sadiesjewels
 - Posts: 48
 - Joined: Mon Mar 10, 2003 2:02 pm
 - Location: N. CA
 - Contact: