I'm looking for some guidance from the Board before investing in a new kiln. I currently am using a Paragon SC-3 (0.28 cu ft) and it's great but much too small. I had a great conversation with Marty at Centre DeVerre this afternoon and am looking at a few different kilns. I'd appreciate your comments, both pros and cons, on them. 
1. Paragon Fusion-10 23"x11"
2. Jen-Ken Kiln, 24"x11", Professional Series
3. Skutt GM-1014, 23.5"x13.5"
Thanks in advance. Sonje
			
			
									
						
										
						Buying a Kiln
Moderators: Brad Walker, Tony Smith
Buying a Kiln
I have just purchased a Paragon Fusion 10 with the Orton 12 key 
My husband is picking it up from the shipping company tomorrow.
I have to work all weekend 8-( so I will not get to play with it at all
But soon as I get it fired up I will let you know.
It is going to be a loooooong weekend.
			
			
									
						
										
						My husband is picking it up from the shipping company tomorrow.
I have to work all weekend 8-( so I will not get to play with it at all
But soon as I get it fired up I will let you know.
It is going to be a loooooong weekend.

Sonje,
I've had the Jen Ken 24" for 4 years and it is great; since then I've added 2 more Jen Kens- the last one was the 41"
Marty will help you and the people at Jen Ken are very helpful. The only repair I had to make was to replace the lid element and their instructions were easy to follow; Judy S gave me good advice, too!
Have fun!
Jo
			
			
									
						
										
						I've had the Jen Ken 24" for 4 years and it is great; since then I've added 2 more Jen Kens- the last one was the 41"
Marty will help you and the people at Jen Ken are very helpful. The only repair I had to make was to replace the lid element and their instructions were easy to follow; Judy S gave me good advice, too!
Have fun!
Jo
Re: Buying a Kiln
Sonje, marty is a great advisor!Sonje Mitchell wrote:I'm looking for some guidance from the Board before investing in a new kiln. I currently am using a Paragon SC-3 (0.28 cu ft) and it's great but much too small. I had a great conversation with Marty at Centre DeVerre this afternoon and am looking at a few different kilns. I'd appreciate your comments, both pros and cons, on them.
1. Paragon Fusion-10 23"x11"
2. Jen-Ken Kiln, 24"x11", Professional Series
3. Skutt GM-1014, 23.5"x13.5"
Thanks in advance. Sonje
 personally i use the jen ken kilns, have a large one about the size you mention above and one of their smaller ones that i started with.  i would highly recommend jen ken and a 12 key controller on it.  the only other thing i can add is if you are thinking at all of doing drop rings, get it 15" deep.
  personally i use the jen ken kilns, have a large one about the size you mention above and one of their smaller ones that i started with.  i would highly recommend jen ken and a 12 key controller on it.  the only other thing i can add is if you are thinking at all of doing drop rings, get it 15" deep.D
- 
				J Campbell
- Posts: 6
- Joined: Fri Mar 14, 2003 2:54 pm
- Location: CA
- Contact:
get the next size up from the largest one you can afford. you'll wish you had in under 6 months.J Campbell wrote:All I can say is get the largest one you can afford. I wish I would have lisen to the advise here myself. Instead, I have one kiln that I don't use and three that I do. Good luck. Jane
also, get a square one. you can put a large square piece in a square kiln. you can't put a large square piece in a round one. for example, the largest square i can put into my 23" round kiln is about 13" on a side, or 10x20" rectangular.