Just ordered three sizes of System 96 frits - need to have COE 96 compatibility with another COE 96 glass I'm fritting out and using.
In reading the System 96 support literature, it looks as though this glass doesn't flow as readily as BE.
Is anyone using this frit for casting? Does it flow well into a more intricately detailed mold or should I do a drip casting?
Thanks
Anyone using System 96 frits?
Moderator: Brad Walker
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact: