Hi
I´m having problems to full fuse two layers of 3/8 in float glass. I know I have to do some kind of dam, but I can´t figure how.
I need to fuse two square layers 18x18 in, and two circular ones, 16 in diameter .
Thanks for any advice
Luiza
Fusing 3/8 float glass
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Fusing 3/8 float glass
LuizaLuiza wrote:Hi
I´m having problems to full fuse two layers of 3/8 in float glass. I know I have to do some kind of dam, but I can´t figure how.
I need to fuse two square layers 18x18 in, and two circular ones, 16 in diameter .
Thanks for any advice
Luiza
I fuse 2 layers of 10mm all the time. Only once did I try a dam and it killed me. The glass hit the dam and curled up then shrunk back and became too small.
I often make the top piece larger than the bottom by it's thickness which makes a rolled edge. The edge is especially good on the circle.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Fusing 3/8 float glass
Hi BertLuiza wrote: Luiza
I fuse 2 layers of 10mm all the time. Only once did I try a dam and it killed me. The glass hit the dam and curled up then shrunk back and became too small.
I often make the top piece larger than the bottom by it's thickness which makes a rolled edge. The edge is especially good on the circle.
What´s the schedule you use? I was wondering about the theory that all glasses likes to be 2 layers high. The glass won´t flow over the shelf and spread?
Please, I really need help with this problem
Thanks a lot
Luiza