Can't find putting a rim on a pot drop in archives? HELP>

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
deborahbur
Posts: 51
Joined: Thu Apr 10, 2003 2:09 pm
Location: Tiverton, Rhode Island
Contact:

Can't find putting a rim on a pot drop in archives? HELP>

Post by deborahbur »

Someone was explaining how to put a rim around a pot drop and I can't find it. Any help would be appreciated.
Thanks
Deborah :D
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

in photos, topic headings like "yet another pot melt" should lead you to it. i'm pretty sure it was in photos, not kiln forming. or look for "all posts by Steve Immerman" -- that's one way to find the thread where he and Randy were showing photos, and the addition of a rim was discussed.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Re: Can't find putting a rim on a pot drop in archives? HELP

Post by Paul Tarlow »

deborahbur wrote:Someone was explaining how to put a rim around a pot drop and I can't find it. Any help would be appreciated.
Thanks
Deborah :D
http://www.warmglass.com/phpBB/viewtopic.php?t=658