Hello,
I have some Gerry's Casting Mix that came with no instructions (I've asked the supplier for the information but haven't heard back from them). The archives here ( I love this board!!) gave some help, but I still have one more question. Do the molds made with this mix need to have a kiln wash applied?
Thanks bunches.
Nancy D.
Becky Bergsma
Posts: 8
Joined: Mon Mar 10, 2003 11:56 pm
Location: Seattle Area
Contact:

Post by Becky Bergsma »

Hi,
This is a one time mold mix. We applied a slip coat to our piece then poured the mold mix over that. No kiln wash needed.

Becky
Nancy D
Posts: 8
Joined: Sun Mar 09, 2003 8:22 pm

Post by Nancy D »

Thanks, Becky, that's what I needed to know.
bye Nancy D.
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Gerry's mold mix.

Post by Jack Bowman »

I took a 2 week class with Gerry last summer and we did some great casting with his mix. He suggested a face coat, somebody else refered to it as a slip coat. I think we are talking about the same thing. the face coat was plaster/silica consistancy of buttermilk. While it's setting mix the Gerry's to milkshake consistancy and pour.

A few links to Gerry's work if your interested.

http://www.theartcollector.com/newcomb.htm

http://www.system96.com/Pages/CastingTu ... llets.html

Jack
PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

jargon?

Post by PDXBarbara »

slip coat = face coat = splash coat??
thx.
Barbara
Barbara Bader
Nancy D
Posts: 8
Joined: Sun Mar 09, 2003 8:22 pm

Post by Nancy D »

Jack,
Thanks so much for the web sites! The second is a great help.
bye Nancy
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

slip coat = face coat = splash coat??

Post by Jack Bowman »

That's the way I understand it.

Jack
Post Reply