I fused a large platter 15x 10 and used two pieces of clear glass on the bottom (instead of one piece). When the firing was done, there was a visable line in the clear glass on the bottom. If I fired hotter would it disappear?
Thanks
Deborah
when fusing two pieces of glass side by side?
Moderators: Brad Walker, Tony Smith
-
deborahbur
- Posts: 51
- Joined: Thu Apr 10, 2003 2:09 pm
- Location: Tiverton, Rhode Island
- Contact:
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: when fusing two pieces of glass side by side?
NOPE.deborahbur wrote:I fused a large platter 15x 10 and used two pieces of clear glass on the bottom (instead of one piece). When the firing was done, there was a visable line in the clear glass on the bottom. If I fired hotter would it disappear?
Thanks
Deborah
Jim