ARTIST MARK/LOGO Q

Post by rodney »

http://www.lhotsky.cz/dsg/k1/t/tk01.jpg

the link above shows the MAKERS MARK, down in the corner, is this cast in, or stamped, when hot, what would keep the mark from distorting during the slump

thanks
rodney
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

Looks like the mark is on the top surface. It could be low fire enamels or a decal that fires on during the slump.

Ron
Lisa Allen
Posts: 212
Joined: Sun Mar 09, 2003 3:23 pm
Location: Memphis, TN
Contact:

Post by Lisa Allen »

Looks like it might be sandblasted on.........at least in the pic of that one.