Adhesives

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Cheryl Wade
Posts: 26
Joined: Sun Mar 23, 2003 5:48 pm
Location: Wales UK

Adhesives

Post by Cheryl Wade »

Can anyone give me advice on the best type of crystal clear adhesive for sticking glass to glass please? I'm making a rectangular vase (25cm x 10cm per side) in fused Artista and Dichroic. I don't want to detract from the glass by using copper foil or lead but have never stuck pieces together before and would like to get it right.
Cheryl
Dani
Posts: 493
Joined: Mon Mar 10, 2003 3:17 pm
Contact:

Post by Dani »

Hxtal or one of its clones is the best and most expensive. It's a museum glue that won't yellow over time.... lots in the archives.