Second question. I slumped this blank into a mold that is 11 inches in diameter and 2 inches deep. The bowl came out 9 1/4 inches in diameter. I assume I slumped too long and the glass started to pool in the bottom. Am I right? I think in my concern to be sure in has slumped all the way to form the bottom, I'm going too far.
Oh yeah, I used Spectrum 96 glass and the over all thickness was 1/4 inch. I followed the recommended schedule from Spectrum for the fuse and the slump for this thickness of glass.
Thanks ahead of time for any help you all give,
Sandpiper, alias Robin