Need basic help on preparing to slump simple project....
Moderators: Brad Walker, Tony Smith
Need basic help on preparing to slump simple project....
I've never slumped before. I want to slump a small vase with some dichroic. Do you FIRST have to fire the glass (fuse) before slumping? Also, how do you determine the exact size and shape to place over the mold? Is there a slumping for idiots tutorial or video I can get my hands on? Thanks.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Need basic help on preparing to slump simple project....
You might check out the tutorial at this site.candala wrote:I've never slumped before. I want to slump a small vase with some dichroic. Do you FIRST have to fire the glass (fuse) before slumping? Also, how do you determine the exact size and shape to place over the mold? Is there a slumping for idiots tutorial or video I can get my hands on? Thanks.