Lonman wrote:Can anyone tell me the firing characteristics and times for fusing with GNA 90?  I am specifically interested in the thicker glass of their's.  It has no bubbles in it and that's what makes it attractive to me.  
Thanks 

 [/img]
Lonman[/url]
 
These days we tend 2 fire very slow
Whatever the glass
I never recomend temp as each kiln is different
I think more about what the glass is doing n past notes
It realy depends on ammount of glass ie layers n the actual set up
Not looked at BE recently
But was the lack of bubbles that attracted me to GNA
ITs actually the Artist range that is compatabble
GNA / Miagra is not sold as compatabble
Although I have used a few tons of it most of the old stock was compatabble
Watch out 4 the darker colours
Not bought any for some 10 or so years although I have about 1 1/2 tons left
Some secret stuff from my private archives 4 U from last year
XXXXXXXXXXXXX
desag antique 75 is now Magera (Europe ) ( in USA its GNA )
XXXXXXXXXXXXXXXXXXXXXXXXXXXXXXX
 
Further to the information that you sent to me from the web-site and our subsequent telephone conversations I am pleased to forward the details that Schott Desag have responded with.
Co-efficient of expansions
Imera  90 - 96      a flat float type glass which is available in 9 colours but is not made compatable 
Antique 75 Sold before 1990   90-96*10-7K-1
Magira 90-96*10-7K-1  The name of Magira in USA is GNA - German New Antique
Artista 94*10-7K1
"Artista is a closer specified version of Magira.  This closer specification guarantees the fuseability of the Artista colours with each other.
Antique 75 is the old name of Magira.  It was/is never made to be compatible.
When people succeed in fusing some Magira colours it happens because they have made test and the coefficient was coincidentally the same.
"
I do hope this addresses the main questions.
Regards
Cathy Salt
XXXXXXXXXXXXXXXXXXXXXXX
 
Brian again
 
all glass in approx 3 - 9 mm    size 1600 x 1500    some bigger
 
http://www.schott.com/desag/english/products/index.html
magira / artista / imera
 
note glass sink Barabra
 
 
http://www.schott.com/english/company/      main site 
 
All the best
 
Brian