What are the do's and dont's r.e. putting iridized glass in with a pot melt?
I know that fusing iridized to iridized doesn't work well. Will iridized in a pot melt also cause problems?
Larry
Pot Melt with Iridized
Moderators: Brad Walker, Tony Smith
-
Larry Lunsford
- Posts: 38
- Joined: Thu May 08, 2003 4:26 pm
- Location: Littleton, CO
- Contact:
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
-
Jerry
Iridized pot melt
Interesting you should ask; I've been considering the same thing. The iridizing will go away at those temps, however, I've been able to keep an iridized look by using a base sheet of iridized and placing the iridized surface DOWN! Don't know why it works but it does.
Jerry
Jerry
Re: Pot Melt with Iridized
[quote="Larry Lunsford"]What are the do's and dont's r.e. putting iridized glass in with a pot melt?
I know that fusing iridized to iridized doesn't work well. Will iridized in a pot melt also cause problems?
one thing i've found when using irid at high temps and then slumping later is the irid tends to stretch and leave a texture and look i don't like if it's on the side against the slumping form
something to keep in mind - haven't played potmelt yet tho'...
D
I know that fusing iridized to iridized doesn't work well. Will iridized in a pot melt also cause problems?
one thing i've found when using irid at high temps and then slumping later is the irid tends to stretch and leave a texture and look i don't like if it's on the side against the slumping form
something to keep in mind - haven't played potmelt yet tho'...
D
-
Edythe Halliday
Pot melt with irid glass
Hi
I have just finished a pot melt with some aventurine green irid [1112-31F] glass in the mix. I went up to 1675 degrees for 1 hour and 15 minutes. You can still see the irid in the finished piece and it shines very nice. I didn't know what would happen but thought I would try as I had lots of scraps. I'm pleased with how it turned out but don't know if other irid glass would do the same.
I will take a picture and see if I can figure out how to send it.
I would go ahead and try the irid.
Edythe
I have just finished a pot melt with some aventurine green irid [1112-31F] glass in the mix. I went up to 1675 degrees for 1 hour and 15 minutes. You can still see the irid in the finished piece and it shines very nice. I didn't know what would happen but thought I would try as I had lots of scraps. I'm pleased with how it turned out but don't know if other irid glass would do the same.
I will take a picture and see if I can figure out how to send it.
I would go ahead and try the irid.