I must be dumb as a box of rocks since I cannot figure this out but here goes. I want to make fused glass picture frames, how on earth do I either attach hanging loops to the back of the glass or attach a zinc or brass channel to the back of the glass frame so that I can use an easel back? For that matter if not using an easel back how do you hold the picture in the frame? I looked in a book that had a few patterns for fused picture frames and there were no instructions.
Thanks a bunch for any help Nanc
Attaching zinc or brass channel to picture frame
Moderators: Brad Walker, Tony Smith
-
Nancy Juhasz
- Posts: 113
- Joined: Sun Mar 09, 2003 10:10 pm
- Location: Ohio
I noticed that in the book "Fusing Made Easy" , it just says "adhere frame to the back." I just purchased the clear acrylic (sp) frames, centered it on back and glued using E6000.
A simple way, but very casual look, would be to fuse two wire loops between the top pieces (similar to the way you do jewelry) to hang with chain.
A simple way, but very casual look, would be to fuse two wire loops between the top pieces (similar to the way you do jewelry) to hang with chain.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Attaching zinc or brass channel to picture frame
I attach the glass insert & channels with 30 min clear epoxy.Nanc wrote:I want to make fused glass picture frames, how on earth do I ... attach a zinc or brass channel to the back of the glass frame so that I can use an easel back?
Don't feel dumb. When I first switched from soldered frames to fused ones I wasn't sure how I was going to attach the easel back channels. So, I found a site where a studio out west made them and sent an e-mail asking if she minded sharing her method. She did mind.
Thank you, Brad, for this board!