Post by Ingrid »

:P A-hah!
I have answered my own qustion but I know others were interested with the answer. It only took me one sleepless night and a month or so to find these decals. For those of you who are interested I found the fusible decals as well as a lot of other glass products at Schlaifer's Enameling Supplies. You can find them at http://www.enameling.com
These decals are made to be fused into the glass, not quite sure if they have the dragonfly or not...but they had some real nice patterns. They weren't too expensive either. Hope this helps someone else besides me.

Thanks...Ingrid :wink: