OK call me cheap, but I just bought some Unique paints from Rainbow Art and they came without temp directions and it is not on their color sheet either. Anyone have experience with them?
I fired red up to 1450(like paradise) and lost most of it, and the rest blackened.
Another question if you don't mind. Anyone use this with an airbrush. I want to bang out some stencil work on float for the tourist season. Let no person walk from my booth emptyhanded!!
I have used these paints on float and go up to 1500. The red turned out fine. I tried an emerald green that turned almost clear. I called and they said to stir and shake and this would cure the problem. i have never tried airbrushing with them.
Jeri Dantzig wrote:OK call me cheap, but I just bought some Unique paints from Rainbow Art and they came without temp directions and it is not on their color sheet either. Anyone have experience with them?
I fired red up to 1450(like paradise) and lost most of it, and the rest blackened.
Another question if you don't mind. Anyone use this with an airbrush. I want to bang out some stencil work on float for the tourist season. Let no person walk from my booth emptyhanded!!
thanks in advance
vineyard Jeri
Ferro Sunshine and Summerday series. 19 mixabe colors. I'm teaching their use in a 3 day workshop preceeding WGWE2.
$200 gets you a complete Sunshine sample set with 50 - 100 grams of each color (mostly 100). See archives for more details. You can also buy any amount of any color with a $100 minimum. They make and sell dozens of mediums. Many other companies buy and resell these items. At Ferro You buy direct from the manufacturer at a good price.