Sharpie residue.
Posted: Sat Sep 27, 2003 11:28 pm
by bskirwin
Does anyone know how to remove silver sharpie marks after firing. I just discovered the silver sharpie to mark on black glass, and assumed it would burn off like black ink does...... Now I have lots of little silver marks all over a kiln load of plates.... is there anyway to get that off now???? Thanks. barbara
Posted: Sat Sep 27, 2003 11:34 pm
by Brock
Sandblasting! Brock
sharpie marks
Posted: Sun Sep 28, 2003 10:12 am
by bskirwin
Borck, thanks for the reply, but the marks are on irid glass fused onto black glass. Do you think that etching cream could remove the silver sharpie marks and not hurt the irid coating, as the cream does not do a good job removeing irid????? Barbara
Posted: Sun Sep 28, 2003 10:13 am
by Brock
I've never tried it . . . Brock
Posted: Sun Sep 28, 2003 1:44 pm
by bskirwin
Well, for anyone out there who is interested, etching cream does remove silver sharpie marks on irid coating without ruining the irid coating...... I just tried it, left it on for ~ 15 minutes and washed it off, scrubbed a little and voila, a sharpie-less look!!!!! Barbara