I like Amazing Glazing line of bits from CR Laurence. I have bought some cheap Chinese bits, but they turned out to be nearly useless to me because they were too short for my tripod drill setup. The AG bits cost a little more and last a lot longer, than their EDD series.Bonnie Rubinstein wrote:I started with the base being single thick, then added on layers, so it became DT..except in a few areas.
I have had luck with the DT to start with, and if it were not for the weight, I would have used DT for this as well. But then I would have added more glass, making it very thick, and for this fixture, I wanted it to be a little lighter. I think I should have added enough glass to make the whole piece DT, consistently.
.. and Bert, if you have a good source for hollow core bits that LAST, please inform..
thanks!