Using spectrum cullet for pate de verre

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Using spectrum cullet for pate de verre

Post by Kevin Midgley »

if the bucket was made of polyethylene, any bits would float however please don't just pour down the drain as those microbits are really hard to get rid of from the environment. Plastic filled fish sounds really appetizing. :mrgreen:
Jordan Kube
Posts: 18
Joined: Sun Oct 01, 2006 10:40 pm
Location: Seattle

Re: Using spectrum cullet for pate de verre

Post by Jordan Kube »

No problem.